Borealis Borcoat™ BB700E-7032 Polypropylene Compound for Steel Pipe Coating Applications
Subcategory: Polypropylene; Thermoplastic
Material Notes: Borcoat BB700E-7032 is a grey colored high impact polypropylene. This product is especially designed for direct extrusion of syntactic PP with high thermal insulations capacity and high compression strength.Borcoat BB700E-7032 is recommended as thermal insulation for offshore deep water flow lines. Information provided by the Manufacturer.