Borealis Borcoat™ EA165E Elastomer Modified Polypropylene for Extrusion
Subcategory: Polypropylene; Thermoplastic
Material Notes: Borcoat EA165E is an elastomer modified compound, based on a high molecular weight copolymer. The elastomer modification gives excellent low temperature impact resistance.Borcoat EA165E is recommended for sheet, pipe extrusion, pipe coating and thermoforming of industrial parts, either as such or as a coextruded layer. It is suitable for applications requiring excellent low temperature performance. Information provided by the Manufacturer.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Notched
- Front Barrel Temperature
- Die Temperature
- Melt Temperature
- Head Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|