Borealis Borecene Compact™ RM8406 Black Linear Polyethylene for Rotational Molding
Subcategory: Polyethylene; Thermoplastic; MDPE
Material Notes: Borecene Compact RM8406 is a third generation linear medium density black polyethylene for rotational molding. The narrow molecular weight imparted through metallocene catalyst technology provides an ideal balance of flow and physical properties. Borecene Compact RM8406 is a black version of Borecene RM8403, suitable for diesel fuel tanks. Borecene Compact RM8406 is delivered as new technology powder.Information provided by the Manufacturer.
| Available Properties |
- Density
- ESCR 10% Igepal®
- Melt Flow
- Tensile Strength @ Yield
- Flexural Modulus
- Dart Drop Total Energy
- Dart Drop
- Deflection Temperature at 0.46 MPa (66 psi)
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|