Borealis Borecene™ RM8342RC Linear Polyethylene for Rotational Molding
Subcategory: Polyethylene; Thermoplastic; MDPE
Material Notes: Borecene RM8342RC is a third generation linear medium density natural polyethylene for rotational molding. Borecene RM8342RC is a special grade, which has passed many rigorous tests and can be considered as a possible replacement for crosslinkable polyethylene in many applications. The narrow molecular weight distribution imparted through metallocene catalyst technology provides an ideal balance of flow and physical properties. Borecene RM8342RC is delivered as pellets.Borecene RM8342RC can be considered as a possible replacement for crosslinkable products in rotational molding such as fuel tanks and tanks. Information provided by the Manufacturer.
| Available Properties |
- Density
- ESCR 10% Igepal®
- Melt Flow
- Tensile Strength @ Yield
- Flexural Modulus
- Dart Drop Total Energy
- Dart Drop
- Deflection Temperature at 0.46 MPa (66 psi)
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|