Borealis Bormed™ HD850MO Polypropylene Copolymer for Healthcare Applications
Subcategory: Polypropylene; Thermoplastic
Material Notes: Bormed HD850MO is a medium melt flow rate polypropylene homo polymer using the Borealis Nucleation Technology (BNT). This provides a polypropylene with excellent dimensional stability and its high crystallization temperature allows for reduced cycle time and increased output. Products made from Bormed HD850MO are characterized by excellent clarity and balanced stiffness/impact properties. Due to the high HDT-value, products made from this grade be steam-sterilized (121°C during 20 minutes).Information provided by the Manufacturer.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Tensile Modulus
- Charpy Impact, Notched
- Impact Test
- Deflection Temperature at 0.46 MPa (66 psi)
- Middle Barrel Temperature
- Die Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|