Borealis Bormed™ HE7541-PH HDPE for Healthcare Applications
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: Bormed HE7541-PH is a bimodal, natural, high-density polyethylene produced by the Borstar PE technology. Bormed HE7541-PH combines low volatiles with high Environmental Stress Crack Resistance (ESCR) and superior flow properties as well as good impact strength and toughness even at low temperatures.Bormed HE7541-PH is recommended for injection molding of caps and closures, pharmaceutical and diagnostic packaging, and IBM containers. Information provided by the Manufacturer.
| Available Properties |
- Density
- ESCR 10% Igepal®
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Yield
- Tensile Modulus
- Tensile Impact Strength
- Deflection Temperature at 0.46 MPa (66 psi)
- Melt Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|