Borealis Bormed™ HF840MO Polypropylene Homopolymer for Medical Applications
Subcategory: Polypropylene; Thermoplastic
Material Notes: Bormed HF840MO is a polypropylene homopolymer intended for injection molding and is modified with an internal lubricant for products requiring a low surface friction (e.g. two-part syringes).Bormed HF840MO is used in medical devices such as syringe barrels, needle covers, catheter connections, screw caps and closures, and medical valves. Information provided by the Manufacturer.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Tensile Modulus
- Charpy Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Melt Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|