Borealis Bormod™ HF955MO Polypropylene Homopolymer for Injection Molding
Subcategory: Polypropylene; Thermoplastic
Material Notes: Bormod HF955MO is a high modulus polypropylene homopolymer. Bormod HF955MO is especially developed within the proprietary Borstar technology. The grade utilizes the unique Borstar reactor design capabilities for high crystallinity polypropylene production in combination with the specific Borstar nucleation technology. This combination gives Bormod HF955MO an unique balance of properties for high speed injection molding technology allowing fast cycle due to high de-molding temperature as well as reduced cooling time.Bormod HF955MO is designed for fast production of articles for packaging and houseware. Examples include containers and products with medium to long flow lengths, houseware goods for ambient temperature use, rectangular and flat products, caps and closures with integral hinges, and products with thicker wall sections requiring short cycle time. Information provided by the Manufacturer.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength @ Yield
- Elongation at Yield
- Tensile Modulus
- Charpy Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Melt Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|