Borealis Borpact™ SE920MO Polypropylene Homopolymer for Injection Molding
Subcategory: Polypropylene; Thermoplastic
Material Notes: Borpact SE920MO is a high impact and transparent polypropylene. Borpact SE920MO is a new generation polypropylene having properties that were earlier not possible to combine. Borpact SE920MO offers an impact normally reached with heterophasic copolymers, but where heterophasic copolymers are opaque. It is transparent.Borpact SE920MO is designed for fast production of articles for packaging and houseware. Examples of products include containers, houseware goods, transparent storage crates and boxes, transparent crates and boxes for industrial handling systems, transparent packaging where high impact is needed, and technical articles where transparency and impact is needed. Information provided by the Manufacturer.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength @ Yield
- Elongation at Yield
- Tensile Modulus
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Notched
- Impact Test
- Deflection Temperature at 0.46 MPa (66 psi)
- Haze
- Melt Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|