Borealis Borseal™ TD210BF Terpolymer for BOPP Film Applications
Subcategory: Polypropylene; Thermoplastic
Material Notes: Borseal TD210BF is a C2/C4 terapolymer film resin especially developed for use as sealing layers in coextruded BOPP film (manufactured on stenter frame and double bubble film process).Borseal TD210BF is especially developed for use as sealing layers in coextruded BOPP film (manufactured on Stenter frame and double bubble film processes). Information provided by the Manufacturer.
| Available Properties |
- Melt Flow
- Flexural Modulus
- Heat Seal Strength Initiation Temperarture
- Melting Point
- Vicat Softening Point
|
|
|
|
| Property Data |