Borealis Borsoft™ SD200CF High Impact Polypropylene Random Heterophasic Copolymer for Cast Film
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Borsoft SD200CF is a very soft random heterophasic copolymer, suitable for use on chill roll process. The product combines unique softness with outstanding mechanical properties making it the ideal solution for mono and coex film design.Borsoft SD200CF is especially suitable for stationery folders, food/textile packaging, technical films, property modification in other applications fields, substitution of other plastics, and hygienic films Information provided by the Manufacturer.
| Available Properties |
- Density
- Thickness
- Melt Flow
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Flexural Modulus
- Secant Modulus, MD
- Secant Modulus, TD
- Impact
- Impact Test
- Melting Point
- Vicat Softening Point
- Haze
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|