Borealis Borsoft™ SF203CF Soft Polypropylene Copolymer for Extrusion Coating
Subcategory: Polypropylene; Thermoplastic
Material Notes: Borsoft SF203CF is a new statistic-heterophasic propylene-ethylene copolymer suitable for coating applications. Its polymer structure permits perfect adhesion to certain products. According to the application, Borsoft SF203CF should be used preferably in blends with PP with high melt strength (HMS).Borsoft SF203CF is specially suitable for sealing layer, textile back sheet, breathable compounds, and soft coating. Information provided by the Manufacturer.
| Available Properties |
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|