Borealis Borstar® HE3494-LS Dark Blue High Density Polyethylene for Drinking Water Pipes
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: Borstar HE3494-LS is a yellow-orange, cadmium free, high density polyethylene compound classified as a MRS 10.0 material (PE100) produced with the advanced Borstar technology. It includes a combination of pigments and stabilizers to ensure long-term, UV-resistance, and resistance to gas condensate. It also shows excellent resistance to rapid crack propagation and slow crack growth.Borstar HE3494-LS is recommended for pressure pipe systems in the applications field of drinking water and natural gas, and gives good processing properties and low sagging in thick-walled pipes. Information provided by the Manufacturer.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Break
- Tensile Modulus
- Front Barrel Temperature
- Die Temperature
- Melt Temperature
- Head Temperature
- Resistance to Papid Crack Propagation, BAR
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|