Borealis Borstar® HE6063 Natural Bimodal HD Polyethylene Compound for Jacketing of Communication and Power Cables

 

Subcategory: Polyethylene; Thermoplastic; HDPE

Material Notes:
Borstar HE6063 is a natural, colorable, bimodal, high-density polyethylene compound, produced using the Borstar process, for jacketing of power and telecommunications cables. It is characterized by its tailor-made properties important in jacketing applications i.e. low shrink back, excellent stress crack resistance, and wide processing window. Borstar HE6063 contains a well dispersed UV-stabilizer in sufficient amount to ensure excellent weathering resistance, corresponding to minimum 15 years exposure in continental European climate.

Borstar HE6063 meets the applicable requirements as below when processed using sound extrusion practice and testing procedure.

Information provided by the Manufacturer.

Available Properties
  • Density
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength @ Yield
  • Elongation at Yield
  • Flexural Modulus
  • Electrical Resistivity
  • Dielectric Strength
  • Brittleness Temperature
  • Pressure Test at High Temp
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。