Borealis Borstar® ME3440 Black Medium Density Polyethylene for Pressure Pipes

 

Subcategory: Polyethylene; Thermoplastic; MDPE

Material Notes:
Borstar ME3440 is a black, bimodal medium density polyethylene compound classified as a MRS 8.0 material (PE80), with optimum balance between flexibility and strength, produced with the advanced Borstar technology. Well dispersed carbon black gives outstanding UV resistance. Long-term stability is ensured by an optimized stabilization system.

Borstar ME3440 is recommended for pressure pipe systems in the application fields of drinking water, natural gas, pressure sewerage, relining, sea outfall and industrial, particularly where flexibility and coilability is of importance. It also shows excellent resistance to rapid crack propagation and slow crack growth. Thanks to the structure, it gives outstanding extrudability, compared to conventional PE80 products.

Information provided by the Manufacturer.

Available Properties
  • Density
  • ESCR 10% Igepal®
  • Carbon Black Loading
  • Melt Flow
  • Tensile Strength @ Yield
  • Elongation at Break
  • Elongation at Yield
  • Tensile Modulus
  • Charpy Impact, Notched
  • Brittleness Temperature
  • Front Barrel Temperature
  • Die Temperature
  • Melt Temperature
  • Head Temperature
  • Resistance to Papid Crack Propagation, BAR
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。