Borealis Borstar® ME6053 Black Bimodal MD Polyethylene Compound for Jacketing of Communication and Power Cables
Subcategory: Polyethylene; Thermoplastic; MDPE
Material Notes: Borstar ME6053 is a natural, bimodal medium-density polyethylene compound produced using the Borstar process. It is characterized by its tailor made properties important in jacketing applications, i.e. very low shrink back, excellent stress crack resistance and wide processing window. Borstar contains a well dispersed UV-stabilizer in sufficient amount to ensure excellent weathering resistance, corresponding to a minimum 15 years exposure in continental European climate.Information provided by the Manufacturer.
| Available Properties |
- Density
- ESCR 10% Igepal®
- Melt Flow
- Hardness, Shore D
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Electrical Resistivity
- Dielectric Strength
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|