Borealis Casico™ FR4802 Non-Halogen Flame Retardant Insulation/Jacketing Compound

 

Subcategory: Polyolefin; Thermoplastic

Material Notes:
Borstar FR4802 is a natural, thermoplastic polyolefin compound designed for flame retardant low voltage wire insulation and jacketing. As such, FR4802 offers a unique combination of good extrusion properties with a non-halogen flame retardant. FR4802 is specifically formulated for use in areas sensitive to smoke, corrosive fumes and toxic combustion products. Its flame retardant properties are conferred by a patented combination of inorganic filler and a novel, char-forming additive. FR4802 is readily pigmented to a variety of colors using standard wire & cable color concentrates designed for thermoplastic or crosslinked polyethylene. UV weather resistance is obtainable by the addition of a suitable carbon black or UV additive.

Borstar FR4802 is intended to be used as a 90°C rated jacket for power cables, flexible cords and building wires. In addition it may also be used as a superior insulation or jacketing compound in PVC replacement applications. For most cable constructions FR4802 has sufficient flame retardant properties to satisfy single wire horizontal and European vertical burning flame tests. It is stabilized for use in contact with copper.

Information provided by the Manufacturer.

Available Properties
  • Density
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength @ Yield
  • Elongation at Yield
  • Flexural Modulus
  • Electrical Resistivity
  • Dielectric Strength
  • Dielectric Breakdown
  • Dissipation Factor, Low Frequency
  • NBS Smoke Density
  • Oxygen Index
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Die Temperature
  • Head Temperature
  • Avergage Rate of Heat Release, kW/m^2
  • CO, kg/dm^3
  • CO2, kg/dg^3
  • Corrosivity of Combustion Fumes, uS/cm
  • Heat of Combustion, MJ/dm^3
  • Ignition Time, sec
  • Insulation Resistance Megaohm -cm
  • Maximum Rate of Heat Release, kW/m^2
  • Pressure Test at High Temp, %
  • Smoke Obscuration, m^2/dm^3
  • Time to Dm (max) min
  • Time to Dm (max), min
  • Water Absorption, mg/cm2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。