Borealis Daplen™ AK4504 TPO Compound
Subcategory: TPO; Polypropylene; Thermoplastic
Material Notes: Daplen AK4504 is a 30% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen AK4504 is a material with excellent impact/stiffness ratio. Thanks to its low thermal expansion this material is suitable to mold parts requiring low change of dimensions over a broad temperature range. The product is optimized to give good surface aesthetics.Daplen AK4504 is designed for acoustic applications, climate control housing, and cowl vent grill Information provided by the Manufacturer.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Melt Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|