Borealis Daplen™ EG102AI Polypropylene Compound 15% Mineral Filled
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Daplen EF102AI is a 15% mineral filled polypropylene compound intended injection molding. EG102AI is an easy flow grade, specially developed for the car industry. Daplen EF102AI has been developed for interior parts where high scratch resistance and excellent flowability is a necessity, including door cladding and door insert. Information provided by the Manufacturer.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Ball Indentation Hardness
- Tensile Strength @ Yield
- Elongation at Yield
- Flexural Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Melt Temperature
- Mold Temperature
- Emissions, ug C/g
- Fogging %
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|