Borealis Daplen™ FS65T20 Polypropylene Compound 20% Mineral Filled, Detergent Resistant
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Daplen FS65T20 is a 20% mineral filled polypropylene compound intended for injection molding. FS65T20 has been developed especially for applications requiring high detergent resistance and heat stability. FS65T20 has well balanced mechanical properties, medium flow rate and good processability and its tested and approved according to UL94 HB. Daplen FS65T20 has been developed for washing machine parts, dishwasher components, and household appliances. Information provided by the Manufacturer.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Ball Indentation Hardness
- Tensile Strength @ Yield
- Elongation at Yield
- Flexural Modulus
- Charpy Impact Unnotched
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Melt Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|