Borealis Daplen™ KB4436 TPO Compound
Subcategory: TPO; Polypropylene; Thermoplastic; Polymer
Material Notes: Daplen KB4436 is a 30% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen KB4436 is a material with excellent impact/stiffness ratio. Thanks to its low thermal expansion this material is suitable to mold parts requiring low change of dimensions over a broad temperature range. The product is optimized to give good surface aesthetics.Daplen KB4436 has been developed for body side moldings, rocker panels, and window frames. Information provided by the Manufacturer.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Shrinkage
- Melt Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|