Borealis Daploy™ SF203HMS High Melt Strength Polypropylene for Extrusion Coating
Subcategory: Polypropylene; Thermoplastic
Material Notes: Daploy SF203HMS resin is a statistic-heterophasic-propylene-ethylene copolymer modified with a polypropylene based structurally isomeric polymer which combines a significantly increased melt strength with largely improved drawability of the polymer melt. Thus, the material is generally characterized by improved processability in polymer forming technologies where stretching flows occur.Daploy SF203HMS is a very versatile coating grade for coating and lamination of various papers, paperboards, plastic films and foils. Daploy SF203HMS has excellent adhesion against OPP, woven PP cloth and PP based nonwovens. Information provided by the Manufacturer.
| Available Properties |
- Density
- Melt Flow
- Neck In
- Coating Weight
- Tensile Modulus
- Charpy Impact, Notched
- Melting Point
- Vicat Softening Point
- Middle Barrel Temperature
- Front Barrel Temperature
- Die Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|