Borealis Steripeel™ WD165CF PO Compound for Sterilisable Peelable Film Applications
Subcategory: Thermoplastic
Material Notes: Steripeel WD165CF is a non-formulated film resin, specially developed for the manufacturing of unoriented peelable cast films on chill roll process.Steripeel WD165CF is suitable for various peelable applications including pre-cooked food packaging, retort food packaging, instant food packaging, dessert food packaging, lamination film, retort pouches, and lidding film. Information provided by the Manufacturer.
| Available Properties |
- Density
- Melt Flow
- Flexural Modulus
- Melting Point
- Vicat Softening Point
|
|
|
|
| Property Data |