Borealis Superclean™ LR4201S Crosslinkable Polyethylene Insulation for Medium and High Voltage Power Cables
Subcategory: Polyethylene; Thermoplastic; LDPE
Material Notes: Superclean LR4201S is a Superclean crosslinkable low density polyethylene (XLPE) for medium and high voltage power cable insulation. The formulation of LR4201S provides an optimum combination of good extrudability and electrical properties. LR4201S is natural in color.LR4201S has been specifically developed for medium and high voltage power cables. Because it is a Superclean material, LR4201S is suitable for use in high voltage cables rated up to 161 kV. Information provided by the Manufacturer.
| Available Properties |
- Density
- ESCR 100% Igepal®
- ESCR 10% Igepal®
- Melt Flow
- Degree of Crosslinking
- Hardness, Shore D
- Tensile Strength @ Yield
- Elongation at Yield
- Tensile Set
- Electrical Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor, Low Frequency
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|