Borealis Visico™ LE4421/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation

 

Subcategory: Polyethylene; Thermoplastic; LDPE

Material Notes:
Visico LE4421/LE4437 is a natural, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination of a Visico base material, LE4421, and a tin catalyst masterbatch, LE4437 provides a highly scorch retardant compound with excellent thermal stability. LE4421/LE4437 contains a patented scorch retardant additive (SRA) that increases the processing window for a moisture crosslinking compound and minimizes the tendency for premature crosslinking in the extruder, head or die. LE4437 should be added to LE4421 directly in the extruder hopper by dry blending at a ratio of 5 parts suitable antioxidants, a metal passivator and a metal deactivator. Properly mixed, during the extrusion process, LE4421/LE4437 exhibits excellent thermal stability to oxidation.

LE4421/LE4437 is recommended for use as insulation for low voltage control cables and power cables up to 6 kV in rating.

Information provided by the Manufacturer.

Available Properties
  • Density
  • Melt Flow
  • Deformation
  • Tensile Strength @ Yield
  • Elongation at Yield
  • Electrical Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor, Low Frequency
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Die Temperature
  • Head Temperature
  • Horizontal Flame Test
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。