Borealis Visico™ LE4421/LE4460/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation
Subcategory: Polyethylene; Thermoplastic; LDPE
Material Notes: Visico LE4421/LE4460/LE4437 is a natural, halogen-based, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination of the Visico LE4421 base resin, along with the LE4460 brominated flame retardant masterbatch and the LE4437 tin catalyst masterbatch provides a highly scorch retardant compound with excellent thermal stability and good flame properties. LE4421/LE4460/LE4437 contains a patented scorch retardant additive (SRA) that increases the processing window for a moisture crosslinking compound and minimizes the tendency for premature crosslinking in the extruder head or die.LE4421/LE4460/LE4437 is recommended for use as insulation for low voltage control cables and power cables up to 6 kV in rating. Information provided by the Manufacturer.
| Available Properties |
- Density
- Melt Flow
- Deformation
- Tensile Strength @ Yield
- Elongation at Yield
- Electrical Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor, Low Frequency
- Middle Barrel Temperature
- Front Barrel Temperature
- Die Temperature
- Head Temperature
- Horizontal Flame Test
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|