Borealis Xmod™ BG055AI High Stiffness Polypropylene for Injection Molding Applications
Subcategory: Polypropylene; Thermoplastic
Material Notes: Xmod BG055AI is a high melt flow polypropylene with increased crystallinity, intended for injection molding. Xmod BG055AI is a very easy flowing material with a good balance between impact strength and stiffness. The material provides high surface quality.Xmod BG055AI is especially designed for air duct systems, climate control units, back-injection molding, and parts requiring high aesthetic surface finish. Information provided by the Manufacturer.
| Available Properties |
- Density
- Melt Flow
- Ball Indentation Hardness
- Tensile Strength, Yield
- Tensile Modulus
- Flexural Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Shrinkage
- Gloss
- Melt Temperature
- Mold Temperature
- Emissions, ug C/g
- Fogging, mg
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|