Borealis Xmod™ GB305HP High Performance Glass Fiber Reinforced Grade

 

Subcategory: Polypropylene; Thermoplastic; Polymer

Material Notes:
Xmod GB305HP is reinforced with 35% chemically coupled glass fibers and based on a specific Polymer matrix material that is bringing excellent mechanical properties (biaxial impact behavior) as well as a very good stiffness at higher temperatures. The grade is equipped with an extraordinary long-term high heat stabilization package.

Xmod GB305HP has been developed especially for the automotive market for applications that require high mechanical strengths at high service temperatures e.g. for parts under the bonnet: air intake manifold, parts for cooling system, and technical components exposed to high heat over longer time.

Information provided by the Manufacturer.

Available Properties
  • Density
  • Melt Flow
  • Spiral Flow
  • Tensile Strength, Yield
  • Tensile Strength, Yield at Elevated Temperature
  • Elongation at Break
  • Elongation at Break at Elevated Temperature
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Strength
  • Charpy Impact Unnotched
  • Charpy Impact, Unnotched Low Temp
  • Charpy Impact, Notched
  • Impact Test
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Vicat Softening Point
  • Shrinkage
  • Gloss
  • Melt Temperature
  • Mold Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。