Borealis Xmod™ GB305HP High Performance Glass Fiber Reinforced Grade
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Xmod GB305HP is reinforced with 35% chemically coupled glass fibers and based on a specific Polymer matrix material that is bringing excellent mechanical properties (biaxial impact behavior) as well as a very good stiffness at higher temperatures. The grade is equipped with an extraordinary long-term high heat stabilization package.Xmod GB305HP has been developed especially for the automotive market for applications that require high mechanical strengths at high service temperatures e.g. for parts under the bonnet: air intake manifold, parts for cooling system, and technical components exposed to high heat over longer time. Information provided by the Manufacturer.
| Available Properties |
- Density
- Melt Flow
- Spiral Flow
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Elongation at Break at Elevated Temperature
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Charpy Impact Unnotched
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Impact Test
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Shrinkage
- Gloss
- Melt Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|