Borealis Xmod™ K65G2 20% Glass Fiber Reinforced Polypropylene Compound
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Xmod K65G2 is a 20% glass fiber reinforced grade intended for injection molding. Xmod K65G2 has been developed especially for the car industry, to be used UTB parts. Xmod K65G2 offers good balance in stiffness/impact strength.Xmod K65G2 has been designed for automotive UTB parts. Information provided by the Manufacturer.
| Available Properties |
- Density
- Melt Flow
- Ball Indentation Hardness
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Melt Temperature
- Mold Temperature
- Fogging, mg
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|