Borealis Xmod™ MC55 High Crystalline Polypropylene Copolymer
Subcategory: Polypropylene; Thermoplastic
Material Notes: Xmod MC55 is a HCPP intended for injection molding of automotive interior parts. Xmod MC55 has an excellent balance between impact strength and stiffness as well as good surface quality.Xmod MC55 has been designed for pillar trims, door panels and pockets, and central consoles. Information provided by the Manufacturer.
| Available Properties |
- Density
- Melt Flow
- Ball Indentation Hardness
- Tensile Strength, Yield
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Shrinkage
- Melt Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|