BorsodChem ONGROSTYR F-I Expandable Polystyrene (EPS)
Subcategory: Polystyrene; Thermoplastic
Material Notes: ONGROSTYR F-I is an expandable, flame-retardant styrene homopolymer, produced by suspension polymerization. The product meets the requirements of DIN 4102 and of B1 class of building materials, i.e. "low inflammability grade".Field of application: ONGROSTYR F-I is suitable for traditional and vacuum molded processing. The minimum apparent density of the end-product is 20 kg/m3. This type is recommended for industrial packaging with 5-10 mm thickness, and decorative panels. It is not for food packaging, when it is in direct contact with the food. Information provided by BorsodChem Rt.
| Available Properties |
- Apparent Bulk Density
- Particle Size
- Viscosity
- Blowing agent content(pentane),%
- Residual Monomer Content max %
- Water Content, %, max
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|