BorsodChem ONGRONOX EHP 75 D peroxide-type initiator
Subcategory: Polymer
Material Notes: Chemical name: Bis-(2-ethylhexyl)-peroxi-dicarbonate. Mol.wt: 346.5g/mol. Active oxygen content: 4.62 %. Deflegmation material: isododecane. Major decomposition products: carbon-dioxide, 2-ethyl-hexanol.Field of application: ONGRONOX EHP 75D is an initiator for ethylene, vinyl chloride, acrylates etc. polymerization and copolymerization. Information provided by BorsodChem Rt.
| Available Properties |
- Density
- Molecular Weight
- Flash Point
- Oxygen Index
- Hydrolizable chlorine
- Peroxide, %
|
|
|
|