BorsodChem ONGRONOX INP 75 D peroxide-type initiator
Subcategory: Polymer
Material Notes: Chemical name: Bis-(3,5,5-trimethyl-hexanoyl)-peroxide, or Di-isononanoyl-peroxide. Mol.wt: 314.50 g/mol. Active oxygen content: 5.09 %. Deflegmation material: isododecane. Major decomposition products: carbon-dioxide, 3,3,5-trimethyl-hexanoic acid, 2,4,4-trimethyl-pentane, 2,2,4,7,9,9-hexamethyl-decane, 2`,4`,4`-trimethyl-pentil-3,5,5-trimethyl-hexanoate.Field of application: ONGRONOX INP 75D is an initiator for ethylene, vinyl chloride, vinylidenechloride, vinyl-acetate, acrylates etc. polymerization and copolymerization. Information provided by BorsodChem Rt.
| Available Properties |
- Density
- Molecular Weight
- Flash Point
- Oxygen Index
- free acid content as isononanoic acid, max, %
- Hydrolizable chlorine
- Peroxide, %
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|