BorsodChem ONGRONAT CL-27 MDI Isocyanate
Material Notes: Description of product: It is a carbo-diimide modified 4,4`-diphenyl-methane-diisocyanate.Field of application: With suitable polyols it can be used as isocyanate component for producing microcellular elastomers, RIM elastomers, coatings and casting elastomers. Together with high molecular weight and reactive polyols it is suitable for producing prepolymers which can be used for manufacturing flexible and semi-flexible integral foams. Information provided by BorsodChem Rt.
| Available Properties |
- Viscosity
- Hydrolizable chlorine
- NCO Content, wt%
|
|
|
|