Accpro® 9934 Enhanced Polypropylene
Subcategory: Polypropylene; Thermoplastic; Polymer
Key Words: High Stiffness, Nucleated, Antistatic, High Surface Hardness, Stain Resistance
Material Notes: Suggested fabrication methods: Injection molding Features: High stiffness, Nucleated, Antistatic, High surface hardness, Stain resistance Complies with FDA specification, Title 21, CFR 177.1520. Typical applications: Compounding, Automotive components Typical property data below from injection molded samples.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|