BP Amoco ACCPRO® 9119X Extrusion Grade Polypropylene
Subcategory: Polypropylene; Thermoplastic
Material Notes: Discontinued 1999; Accpro® 9117 or Acclear® 6219 are suggested alternatives. Sheet Extrusion. Features: Clarity, High stiffness, High heat resistance, Improved MVTR.Typical property data below from injection molded samples. Data provided by BP Amoco Polymers, Inc.