BP Amoco 7239 Polypropylene Homopolymer
Subcategory: Polypropylene; Thermoplastic
Material Notes: Discontinued 1999; Acclear® 8449 is a suggested alternative.Injection Molding. Features: Clarified, Antistatic. Applications: Clear packaging Typical property data below from injection molded samples. Data provided by BP Amoco Polymers, Inc.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
|
|
|
|