Brandenburger BRA_GLA 3 Thermal Insulation Board
Subcategory: Thermoset; Polymer
Material Notes: A material with high quality glass fibre fabric and roving layers in conjunction with heat resistant EP matrix, which provides a thermal protection with excellent compressive and flexural strength, as well as high interlaminar shear strength. Well suited for applications in heated presses for processing ultra-high-molecular PE, for special-purpose high-stressed piston and press table insulations. Information provided by Brandenburger Isoliertechnik GmbH&Co.
| Available Properties |
- Density
- Water Absorption
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- CTE, linear 20°C
- Thermal Conductivity
- Maximum Service Temperature, Air
|
|
|
|