Brandenburger KV 3 Thermal Insulation Board
Subcategory: Thermoset; Polymer
Material Notes: This material is popular in applications where thermal and mechanical stress occur together. This material is based on a matrix of high temperature resistant polymers and special glass silk fabrics. Typical applications are thermally and mechanically high-stressed heated presses and moulds. Also KV 3 is used to insulate drop forge dies, in the design of soldering masks and in many other applications. Information provided by Brandenburger Isoliertechnik GmbH&Co.
| Available Properties |
- Density
- Water Absorption
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- CTE, linear 20°C
- Thermal Conductivity
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |