Brandenburger AE 2000 N Compensating Inlay
Subcategory: Thermoset; Polymer
Material Notes: This material consists of a pre-impregnated glassfibre mat cured on the press to correct the parallelism in heated presses where unevenness has occurred owing to corrosion and uneven pressure distribution. Information provided by Brandenburger Isoliertechnik GmbH&Co.
| Available Properties |
- Density
- Compressive Strength
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |