Brandenburger Supratherm HT 175 High Temperature Insulation Material
Material Notes: This tightly compressed thermal insulation material with a temperature resistance up to 1000 °C is based on high-grade magnesium silicates, inorganic fibres and binders. Information provided by Brandenburger Isoliertechnik GmbH&Co.
| Available Properties |
- Density
- Water Absorption
- Flexural Strength
- Compressive Strength
- CTE, linear 20°C
- Thermal Conductivity
- Maximum Service Temperature, Air
|
|
|
|