Braskem Symbios® 4101 Polypropylene Film Coextrusion
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Bioriented and conventional film for coextrusion; bioriented and conventional heat sealing film; properties modifier for conventional films; metallizing and lamination process. Information provided by Braskem
| Available Properties |
- Thickness
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Elongation at Yield, MD
- Film Elongation at Yield, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Heat Seal Strength Initiation Temperarture
- Haze
- Gloss
|
|
|
|