Braskem BS 002 HDPE Blow Molding Polyethylene
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes:
Applications: Bottles for medicines, cleaning products, cosmetics, food products and surface-active agents. Information provided by Braskem
| Available Properties |
- Density
- ESCR 100% Igepal®
- Melt Flow
- Hardness, Shore D
- Tensile Strength at Break
- Tensile Strength, Yield
- Flexural Modulus
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |