Braskem LQ 0518/21 AF LLDPE Blown Film Extrusion Polyethylene
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Material Notes: 38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Coextruded film for automatic packaging (FFS). Information provided by Braskem
| Available Properties |
- Density
- Thickness
- Melt Flow
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Coefficient of Friction
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Haze
- Gloss
- Additives
- Minimum Recommended Thickness
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|