Buckeye Polymers BP Flex D6707 TPO
Subcategory: Elastomer, TPE; Thermoplastic
Key Words: Thermoplastic Elastomer, TPE
Material Notes: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a wide service range from -20 degrees C to 120 degrees C, high tear resistance, low density, and good paintability. Information provided by LarSan Chemical Company.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Flexural Modulus
- Tear Strength
|
|
|
|