Buckeye Polymers BP PPC 0212 RReprocessed Polypropylene, Unfilled
Subcategory: Polypropylene; Thermoplastic
Key Words: PP
Material Notes: Blk/White This reprocessed product is successful in applications where cost is a major specification, yet physical characteristics require product performance. Industrial recycled resin compounds are utilized in this mineral reinforced polypropylene product to help meet the wide recycling requirements. Information provided by LarSan Chemical Company.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Ultimate
- Flexural Modulus
- Izod Impact, Notched
- Gardner Impact
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |