Continental Acrylics CA-945 Clear Impact Modified Acylic Resin
Subcategory: Acrylic; Thermoplastic
Material Notes: Impact modified acrylic resin, extrusion and injection molding Applications: An impact-modified acrylic resin for extrusion and injection molding. This resin offers impact strengths up to six times of general-purpose acrylic resins. It also offers good heat resistance. Information provided by Continental acrylics.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Ultimate
- Izod Impact, Notched
- Impact Test
- Deflection Temperature at 1.8 MPa (264 psi)
- Transmission, Visible
|
|
|
|