Shell Carilon® DP R1000 Polyketone, Development Product
Subcategory: Polyketone; Thermoplastic
Material Notes: Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON® Thermoplastic Polymer DP R1000 is a high flow developmental engineering polyketone resin from Shell Chemical Company. Due to its balance of stiffness, toughness, chemical resistance, and easy processing, CARILON Polymer DP R1000 is expected to find application in the appliance, automotive, electrical, and other industries. This high flow, low viscosity polymer should be considered for moldings with long flow paths or thin walls.Data provided by Shell Chemical.
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Izod Impact, Unnotched
- Gardner Impact
- Taber Abrasion, mg/1000 Cycles
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Arc Resistance
- Comparative Tracking Index
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|