Shell Carilon® D26FX100 Polyketone, General-Purpose Extrusion Grade
Subcategory: Polyketone; Thermoplastic
Material Notes: Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26FX100 is a general-purpose extrusion grade with mechanical properties that classify it as an engineering thermoplastic. This grade exhibits high chemical resistance and barrier performance. Moreover, this grade shows a high impact resistance, both at room temperature and at lower temperatures, and good creep performance. CARILON Polymer D26FX100 can also withstand short-term exposure to elevated temperatures.
CARILON Polymer D26FX100 is processable on standard extrusion equipment and may be considered for the production of tubes, industrial hoses, monofilaments, coatings for cable and wire. It is also possible to coextrude CARILON Polymer D26FX100 with other materials, typically to be employed as a barrier layer in containment applications.Data provided by Shell Chemical.
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Melt Flow
- Hardness, Rockwell R
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Izod Impact, Unnotched
- Izod Impact, Notched, Low Temp
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Taber Abrasion, mg/1000 Cycles
- Arc Resistance
- Comparative Tracking Index
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
- Oxygen Index
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|